6713/35 Glossy orange
yellow
| A colorful crystal glaze based on zinc and lithium. Too thick it will run a lot. Spray the glaze thinner near the bottom of the pot. 1260oC with 1/2-3/4 hour at the top temperature. Does not need a slow cooling. Try a second burning. Try also more ferric oxide. |
![]() click for larger |
|