G627
Turquoise silky matt
| A very loved dark turquoise blue glaze. If too thick it will run and be very dry and not good. Works best on very fine porcelain clays. I use a French clay from Limoges. 1260-1280oC with one hour at top temperature. |
![]() |
|
G620, a
variation of G627
|