| Color depends on thickness.
Very thin glaze is gray, fairly thin green and
semi matt. Thicker glaze becomes blue and semi
glossy to glossy with small crystals. 1270oC
with one hour at top temperature. Very good for
incised decoration. Safe glaze. |
| |
|
| potash feldspar NR |
59,40 |
| whiting |
17,50 |
| china clay |
4,66 |
| Albany slip (the real thing) |
7,30 |
| rutile |
7,30 |
| zinc oxide |
1,16 |
| quarts |
1,46 |
| cobalt oxide |
1,46 |
|