My clays: I use K118, a gray white stoneware clay from the Dutch company Vingerling, and PD10, a porcelain clay from the Swedish IFÖ. For special purposes (read turquoise glazes) I use a French porcelain clay from Limoges. Sometimes I also use different brown stoneware clays for Chün and Shino glazes. To 95% I use K118 or PD10. K118 is better for big pots than PD10. Glazes: Short about the recipes: |