Lasse Östman, potter. Stoneware and Porcelain. Glaze list
From this list you can get the recipes without using frames. When you want to go back to this list use your browsers "back". |
REDUCTION: | Glaze No: | Description: |
Celadon and similar: | 92187 | Fat green celadon, both for gray and colored clays |
92058 | Light blue chun, for brown clays | |
Copper red: | 92165 | Glossy clear red, for white and gray stoneware and porcelain |
92166 | Rose, crackled, semi matt, for white and gray stoneware and porcelain | |
92167 | Middle red, darker spots, best on gray stoneware | |
Tenmoku and similar: | 92210a | Traditional tenmoku, works on many clays |
Other reduction: | 92099 | Semi matt to glossy blue |
R626 | Black with brown (or blue) spots, on many clays | |
SH6 | Shino glaze, not for white and gray clays | |
![]() |
||
OXIDATION: | ||
Brown and black: | K 315 | Semi matt, black oilspot |
CR729 | Brownish red with dark spots, for most clays | |
Crystal: | all
crystal glazes best on white porcelain or light gray stoneware clays. |
|
6713kaeg1 | Glossy cobalt blue | |
6713/8 | Glossy yellowish, blue crystals | |
6713/31 | Glossy gray, blue and brown | |
6713/35 | Glossy orange yellow | |
6713/58 | Light blue to turquoise | |
6713/60 | Glossy green and brown | |
C420 | Blue and yellow | |
C426 | Yellow | |
6a5e2 | Semi matt, dark blue | |
6BC | Blue and yellow | |
Zinc Barium: | 5k5v | Silky matt mushroom-colored, not colored clays |
Other oxidation: | H719 | Black and blue with silvery spots |
P72 | Semi matt cobalt green, spots | |
T619 | Silky matt greenish crackle | |
G627/G620 | Turquoise silky matt | |
S419 | Matt/glossy gray, green and blue | |
S422 | Matt golden yellow | |
R626 | Black with blue or brown dots | |
Superimposed: | Coming! | Two or more glazes on top of each other |
More glazes will add!