5. Various Pots (SOLD)

no100
No 100
no91
No 91
no90
No 90
no92
No 92
10x10.gif (55 bytes)
no94
No 94
no97
No 97
no93
No 93
no96
No 96
10x10.gif (55 bytes)
no95
No 95
no102
No 102
no101
No 101
no99
No 99

top

No 90 Big bowl, about 65cm. Glaze 6BC + 6AK. Oxidation
No 91 Bottle vase, about 22cm. Uranium crystal glaze 6k4y8e01. Oxidation
No 92 Bowl, chün glaze, 72058. Reduction
No 93 Cylindrical bowl, superimposed glaze 13/225Co + P2217, Oxidation
   
No 94 Vase, detail. Crackle glaze T619. Oxidation
No 95 Bowl, about 25cm. Copper red. Reduction
No 96 Bowl, about 22cm. Copper red. Reduction
No 97 Bowl, detail. About 35cm. Glaze 6713/58. Oxidation
   
No 99 Urn, about 35cm. Glaze R619. Reduction
No 100 Bowl, about 40cm. Various crystal glazes. Oxidation
No 101 Bowl, about 20cm. Mat crystal glaze 92291. Reduction
No 102
Dome-shaped vase, about 20cm. Crackle glaze T619. Oxidation