Lasse Östman, potter. Stoneware and Porcelain. Exhibition 3
![]()
![]()
Exhibition 1 | Exhibition 2 | Exhibition 4 | Exhibition 5 | Exhibition 6 | Exhibition 7 | Exhibition 8 | Exhibition 9
Glaze Page
| How to buy - Price list | My glaze pictures (macro photos): No 1
| No 2
| Part
1 - Older Pots This first section displays some vases and bowls from 1979-85. The pictures are made from black-and-white photos and then toned brown. All pots are now in private or public collections. |
![]()
Part 2 - New
Pots
This is newly made pots. Some pots may be
not sold. Look for price in the Price List.
![]() |
No 57: Bowl brown and black superimposed glaze. d. 19cm, h. 14cm glaze No: 13/225Co + Basic Albany Glaze oxidation |
![]() |
No 58: Bowl brown superimposed glaze. d. 23cm, h. 12cm glaze No: CR729 + 13/95v, oxidation. |
![]() |
No 59: Bowl brown and black superimposed glaze. d.24cm, h. 16cm glaze No: 13/214 + CR729, oxidation |
![]() |
No 60: Bowl brown, black and grey superimposed glaze. d. 15cm, h.14cm glaze No: 13/225 + P2217, oxidation |
![]() |
No 61: Bowl golden yellow brown glaze. d. 16cm, h. 19cm glaze No: S422, oxidation |
![]() |
No 62: Bowl golden yellow brown glaze. d. 18cm, h. 19cm glaze No: S422, oxidation |
![]() |
No 63: Dish brown, black and grey superimposed glaze d. 34cm, h. 7cm glaze No: 13/225Co + P2217, oxidation |
![]() |
No 64: Bowl red brown and black superimposed glaze. d. 20cm, h. 13cm Glaze No: Inside: 13/225 + 92187, outside: 13/225 + CR729, oxidation |
![]() |
No 65: Wide Bowl red brown glaze with black dots. d. 25cm, h. 7cm Glaze No: F610, oxidation |
| About the pictures in section two: These pictures are made with a digital camera, Casio QV-300. To load quickly they are compressed to JPEG with low quality. Also the bigger ones are compressed the same way. That's why also these pictures are not so sharp. But they will load quickly. |
I hope you enjoyed my pots. |
Exhibition 1
| Exhibition
2 | Exhibition 4 |
Exhibition 5 | Exhibition
6 | Exhibition 7 | Exhibition
8 | Exhibition 9
Glaze Page | How to buy - Price list | My glaze pictures (macro photos): No 1
| No 2