Lasse Östman, potter. Stoneware and Porcelain. Exhibition 1
Exhibition
2 | Exhibition
3 | Exhibition
4 | Exhibition
5 | Exhibition
6 | Exhibition
7 | Exhibition
8 | Exhibition
9
Glaze page |
My Glaze pictures (macro photos): No
1 | No 2
These things are not for sale (sold long time ago) / Clays: K118 or PD10, oxidation 1280oC
![]() |
No 1: Bowl black and brown copper vanadium glaze. d. 16cm, h. 11,5cm glaze No: H719 |
![]() |
No 2: Vase yellowish brown zinc barium glaze. h. about 20cm glaze No: 6ak4 |
![]() |
No 3: Mushroom zinc barium glaze with uranium and cobalt. h. about 16cm. glaze No: 6k4y8e01 |
![]() |
No 4: Garden pot. brown and blue zinc crystal glaze. h. 34cm glaze No: 6ak4g1 |
![]() |
No 5: Miniature bowl brown and blue zinc crystal glaze d. about 6,5cm glaze No: 6a4e2 |
![]() |
No 6: Vase and miniature bowl. glaze based on earthenware clay h. about 30cm/ vase d. about 2,5cm/ miniature |
![]() |
No 7: Miniature bowl (earthenware) golden brown aventurine glaze with borax d. about 4,5cm |
![]() |
No 8: Vase blue and black cobalt vanadium glaze h. about 30cm glaze No: H719x a very unusual glaze with blue, silvery and black dots |
![]() |
No 9: Bowl zinc lithium crystal glaze with manganese d. about 35cm |
![]() |
No 10: Bowl zinc lithium crystal glaze with ferric oxide h. about 28cm |
![]() |
No 11: Bowl nepheline syenit glaze with cobalt and copper d. about 23cm glaze No: p72 |
![]() |
No 12: Vase zinc crystal glaze with cobalt and ferric oxide h. about 22cm glaze No: 6AK |
![]() |
No 13: Bowl crackled feldspar glaze with copper d. about 20cm glaze No: T625 |
![]() |
No 14: Vase zinc barium glaze with uranium h. about 15cm glaze No: 6k4y8 |
![]() |
No 15: Vase zinc barium glaze with cobalt and ferric oxide h. about 28cm glaze No: 6a5e2 |
![]() |
No 16: Bowl and pot barium rich glaze with copper/ feldspar crackle glaze with copper d. about 15cm, bowl h. about 25cm, pot glaze No: G627 / T619 |
![]() |
No 17: Dish lithium crystal glaze with rutile and ferric oxide d. 46cm glaze No: 7/102 |
![]() |
No 18: Dish lithium zinc crystal glaze with cobalt d. 51cm glaze No: 6713kaeg1 |
![]() |
No 19: Bowl zinc crystal glaze with cobalt and ferric oxide d. 29cm |
![]() |
No 20: Bowl zinc lithium crystal glaze with copper and cobalt d. 27cm glaze No: 6713/58x |
About the pictures: These pictures are scanned (flatbed 150 dpi) from old photos (bad and good), and then "repaired" in PhotoShop. To load quickly they are compressed to JPEG with low quality. Also the bigger ones are compressed the same way. That is why also these pictures are not so sharp. |
I
hope you enjoyed my pots. |
Exhibition 2 | Exhibition 3 | Exhibition 4 | Exhibition 5 | Exhibition 6 | Exhibition 7 | Exhibition 8 | Exhibition 9
Glaze page | My Glaze pictures (macro photos): No 1 | No 2