Lasse Östman, potter. Stoneware and Porcelain. Exhibition 4
![]()

Exhibition 1
| Exhibition 2
| Exhibition 3
| Exhibition 5 |
Exhibition 6 | Exhibition
7 | Exhibition 8 | Exhibition
9
Glaze page
There are many crystal glaze pots on exhibition 1 too!
![]() |
No 71: Bowl semi transparent lithium crystal glaze with ferric oxide. d. 16cm, h. 7cm glaze No: 6713/35, oxidation |
![]() |
No 72: Spherical vase blue crystal glaze with cobalt, ferric and manganese oxide. d. about 32cm, h. about 22cm glaze No: 6713kaeg1, oxidation, 1280oC, fired two times (SEK 35000.-) |
![]() |
No 73: Garden pot 1989 blue crystal glaze with cobalt, ferric and manganese oxide. d. 36cm, h. 41cm glaze No: 6713kaeg1, oxidation, 1280oC. |
![]() |
No 74: Bowl violet blue zinc crystal glaze with ferric and cobalt oxide. d. about 35cm, h. about 25cm glaze No: 6AK |
![]() |
No 75: Vase brown crystal glaze with ferric, manganese and nickel oxide. d. about 15cm, h. about 25cm glaze No: 6713/31 |
![]() |
No 76: Same as No 72. |
![]() |
No 77: Bowl blue zinc crystal glaze with ferric and cobalt oxide. d. about 25cm, h. about 15cm glaze No: 6a5e2 |
![]() |
No 78: Dish dark blue crystal glaze with ferric and cobalt oxide. d. about 30cm, h. about 7cm glaze No: c420 |
![]() |
No 79: Bowl Yellow and blue zinc lithium crystal glaze d. about 25cm, h. about 14cm glaze No: 6713/8 |
![]() |
No 80: Bowl yellow and blue zinc lithium crystal glaze d. about 28cm, h. about 15cm glaze No: 6713/8 |
![]() |
No 81: Dish blue white with light yellow crystals. Zink crystal glaze. d. about 30cm, h. about 7cm glaze No: 6713/86 |
![]() |
No 82: Bowl beige and blue crystal glaze with ferric and cobalt oxide. d. about 45cm, h. about 12cm glaze No: 6BC + 6713kaeg1 |
![]() |
No 83: Dish turquoise and blue zink lithium crystal glaze. d. about 32cm, h. about 6cm glaze No: 6713/58 |
![]() |
No 84: Dish yellow green zink crystal glaze with uranium and cobalt. d. about 32cm, h. about 6cm glaze No: 6k4y8e01 |
![]() |
No 85: Bowl blue and yellow crystal glazes d. about 25cm, h. about 16cm glaze No: c420 + 6BC + ?? |
![]() |
No 86: Dish blue crystal glaze d. about 32cm, h. about 7cm glaze No: 6713/8 + ?? |
Exhibition 1
| Exhibition 2
| Exhibition 3
| Exhibition 5 |
Exhibition 6 | Exhibition
7 | Exhibition 8 | Exhibition
9
Glaze page